Customization: | Available |
---|---|
Application: | Aluminum Plastic Film, Pouch Cell Material |
Shape: | Flat |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Consist |
D-EL40H |
||
ON25 |
|||
DL4 |
|||
AL40 |
|||
Improved PPa15 |
|||
Improved PP30 |
|||
Acid modified resin combination, waterproof and acid attacks (Thickness 114µm) |
|||
Thickness |
µm |
Designed |
114 |
Steam Barrier Property 60°C90%RH 336H |
PPm |
Sealing Pressure 1.0MPa |
50↓ |
Initial strength of laminated layers(AL/PPa) |
N/15mm |
11~12 |
|
Initial sealing strength |
N/15mm |
Sealing Pressure 0.5MPa |
70~80 |
190°C 3seconds |
Sealing Pressure 1.0MPa |
85↑ |
|
The electrolyte resistance(Test for sealing into film strength) |
N/15mm |
4.0↑ |
|
60°C 14days |
|||
Electrolyte resistance(Test for sealing into film strength) |
N/15mm |
Sealing Pressure 0.5MPa |
40~50 |
60°C 14days |
Sealing Pressure 1.0MPa |
50~60 |
|
Sealing strength for electrolyte |
N/15mm |
Sealing face pressure 0.5MPa |
80~90 |
190°C 3seconds |
Sealing face pressure 1.0MPa |
80~90 |
|
Punch forming depth |
mm |
Control drape pressure 0.17MPa (Size:80*120mm) |
5.0↑ |