Lithium ion battery materials- Aluminum Laminated Film for Pouch Cell Case GN-alf 113\
This aluminum laminated film (113 um ) is used as casing material for polymer Li-ion battery, detail size can be cutted according your request.
We can provide a full range of lithium battery materials and equipment
1. )full set of lithium battery materials, including:
LiMn2O4, LTO, LiNiMnCoO2(NMC), LiCoO2, Graphite(MCMB)and other cathode&anode battery materials; Aluminum foil, copper foils, battery separator, etc.
2. )full set of lithium battery equipment, for example:
Mixing machine --coating machine--oven--rolling machine--welding machine--slitting / cutting machine --winding machine--sealing machine, etc.
3)full set of lithium battery technology.
We can design the laboratory and production line, according to customer's request.
We have successfully completed lithium battery production line turn key project with Bolivia government, this is the first lithium battery project in South America, for mobile cell phone battery and E-bike battery.
Also Bolivia President attended the opening on Feb 17th, 2014.
Turn-key Project of Li Battery (Lab, Mobile, EV) Production Line Video Link:
http://gelonlib.en.made-in-china.com
What's our advantage:
A: Full set of products chain from lithium ion battery materials, equipment, battery production technology;
B. 10 years lithium ion battery working experiences
C. More than 9 years exporting experiences and 6 years golder supplier in Alibaba
D. Strong teams for markets and agents, and customers all over the world from Asia, American, Europe. Middle East etc;
Choose us means you choose the all-powerful partner for your business
More details please check here:
Bolivia News Videos:
http://gelonlib.en.made-in-china.com
Project Opening:
http://gelonlib.en.made-in-china.com
http://gelonlib.en.made-in-china.com
For more detail pls kindly contact
S: Nancygelon
Consist |
D-EL40H |
ON25 |
DL4 |
AL40 |
Improved PPa15 |
Improved PP30 |
Acid modified resin combination, waterproof and acid attacks
(Thickness 114µm) |
Thickness |
µm |
Designed |
114 |
Steam Barrier Property
60°C90%RH 336H |
PPm |
Sealing Pressure 1.0MPa |
50↓ |
Initial strength of laminated layers(AL/PPa) |
N/15mm |
|
11~12 |
Initial sealing strength |
N/15mm |
Sealing Pressure 0.5MPa |
70~80 |
190°C 3seconds |
Sealing Pressure 1.0MPa |
85↑ |
The electrolyte resistance(Test for sealing into film strength) |
N/15mm |
|
4.0↑ |
60°C 14days |
Electrolyte resistance(Test for sealing into film strength) |
N/15mm |
Sealing Pressure 0.5MPa |
40~50 |
60°C 14days |
Sealing Pressure 1.0MPa |
50~60 |
Sealing strength for electrolyte |
N/15mm |
Sealing face pressure 0.5MPa |
80~90 |
190°C 3seconds |
Sealing face pressure 1.0MPa |
80~90 |
Punch forming depth |
mm |
Control drape pressure 0.17MPa (Size:80*120mm) |
5.0↑ |